Analysis Of Upstream And Offstream Conidtions On Free Surfaces In The Glass Melt By Registration Of Floater Movemtns (In German)

The analysis of flow at free surfaces in glass tank is described. Use of the technique enables the upstream and downstream flow zones to be determined in electrically-heated tanks and the flow rates can be evaluated.