Analysis Of The Mechanical Strength Of Glass Containers (In Italian)

About 3M/tonnes of glass containers are manufactured annually in Italy, which are required to withstand mechanical stress since the forming stage. The stress distribution during production and its service life first taken into account when designing a container - so as to detect weak points and correct them by modifying the containers geometry. In different steps of the production cycle, stress analyses will identify weak points caused by defects, so that appropriate action can be taken. Glass strength issues are briefly reviewed in this paper, and detail is given on the different analyses and tests that can be performed on glass containers, with reference to specific standards. Relevant simplified equations are illustrated, and possible causes of weakening are suggested.

Author
R Dall'Igna
Origin
Stazione Sperimentale, Italy
Journal Title
Rivista Staz Sper Del Vetro 1 2005 5-25
Sector
Container glass
Class
C 4057a

Request article (free for British Glass members)

Analysis Of The Mechanical Strength Of Glass Containers (In Italian)
Rivista Staz Sper Del Vetro 1 2005 5-25
C 4057a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.