Analysis Of Glasses Using Atomic Absorption And Atomic Emission Spectrometry. Part 2. Recommended Procedures Using The Single-Buffer Method With Single Or Multi-Element Calibrations (Italian)

The procedure recommended by Technical Committee 2 of the International Commission on Glass is described.