Analysis Of Glasses, Oxides And Concentration Profiles In Surfaces Or Suraface Films Using High Energy Ions By Secondary Ion Emission (Sims), Photons (Ibsca, Scaniir) And Reflected Ions (Leiss, Heiss). (In German)

Various surface analysis techniques are described and results obtained on glasses and oxides are reviewed briefly.