The Analysis Of Glass Raw Materials And Optical Glasses By The Method Of Infra-Red Absorption Spectroscopy

Infra-red spectra for raw materials and selected optical glasses prepared in the form of tablets pressed in vacuum were determined , the results interpreted, and the practical usefulness of the method discussed.

Author
A Hubert
Origin
Unknown
Journal Title
Szklo I Ceram 22 11 1971 321
Sector
Primary Papers
Class
PP 1317