Analysis Of The Form And Causes Of Iron Bubbles In Brown Glass

One of the common defects of glass is caused by the appearance of visible gaseous stones or bubbles, which can destroy the consistency and optical appearance of the products. This article gives a detailed view on experiments carried out to analyse these bubbles, and how and why they are formed