The Analysis And Control Of Glass And Raw Materials

By means of examples the relations between raw materials and glass composition as well as a comparison of different raw materials in relation to composition, introduction, and effects on the product are all examined. The importance of raw material analysis, the significance of the results and improvements are discussed.