Amorphous Silicon Carbonitride Fibres Drawn From Alkoxide Modified Ceraset

It is shown that the rheology of a silazane-based precursor for a silicon carbonitride ceramic can be radically altered by reacting it with an alkoxide precursor. This modified precursor can be drawn into fibres by a simple process. The fibre-friendly rheology of the modified precursor is ascribed to the creation of linear polymer chains by a reaction between silazanes and alkoxides. The ceramic fibres made by this process have excellent mechanical properties, reaching tensile strengths of 2.8 GPa. Their structure is amorphous.

Author
A Saha Et Al
Origin
University Of Colerado, Usa
Journal Title
J Am Ceram Soc 86 8 2003 1443-1445
Sector
Glass Fibre
Class
GF 370

Request article (free for British Glass members)

Amorphous Silicon Carbonitride Fibres Drawn From Alkoxide Modified Ceraset
J Am Ceram Soc 86 8 2003 1443-1445
GF 370
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.