Aluminoborate Glass-Ceramics With Low Thermal Expansivity

The synthesis and properties of calcium, strontium, and barium aluminoborate glass-ceramics are described.

Author
J F Macdowell
Origin
Corning Inc
Journal Title
J Am Ceram Soc 1990 73 8 2287-2292
Sector
Glass Ceramics
Class
GC 75