Aluminium Release Of Pharmaceutical Glass Containers: Determination By Gfaas In The Extract Solutions And Study Of The Inner Surfaces By Xps And Sims

Aluminium release has been determined for different glass containers for pharmaceutical use after autoclave treatment with distilled water for 60 min at 121 degrees C.