Aluminium Nitride Fibres Synthesized From Alumina Fibres Using Gas-Reduction-Nitridation Method

Aluminium nitride fibres were successfully synthesized from alumina fibres using an NH2-CH3H8 gas mixture as a reduction-nitridation agent. Observation using SEM clearly demonstrated that the morphology of the nitride fibres was exactly the same as that of the raw alumina fibres, retaining the original regular shape and smooth surface. Up to 95% of the starting alumina was converted to aluminium nitride at 1400 deg C within 0.5h via a single-step synthesis process.

Author
T Suehiro Et Al
Origin
Yokohama National University, Japan
Journal Title
Jacs 85 3 2002 715-717
Sector
Glass Fibre
Class
GF 354

Request article (free for British Glass members)

Aluminium Nitride Fibres Synthesized From Alumina Fibres Using Gas-Reduction-Nitridation Method
Jacs 85 3 2002 715-717
GF 354
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
17 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.