Allied Designs Malt Whisky Bottles

Allied Glass has developed a collection of bottles for the new range of Glen Scotia premium single malt whiskies. The bottles have been designed to rejuvenate Glen Scotia as premium single malt while reflecting the style of the distillery and Campbeltown single malts. The three individual bottles, two of which are produced in white flint and one in green glass, are tall and slender in shape giving an elegant feel.