All-Silica Fibres For Ultraviolet Transmission

All-silica fibres are prepared by MCVD and rod-in-tube processes. This paper presents the results of transmission properties and the surface damage threshold of several all silica fibres at the XeCl wavelength (308nm). Transmission loss and the fracture limits of these fibres due to bending are measured.

Author
S Mingwu & G Sijian
Origin
China Building Materials Academy, Beijing
Journal Title
Proc Xvii Icg Vol 5 Beijing 1995 268-272
Sector
Glass Fibre
Class
GF 279

Request article (free for British Glass members)

All-Silica Fibres For Ultraviolet Transmission
Proc Xvii Icg Vol 5 Beijing 1995 268-272
GF 279