All-Electric Forehearth Developments, Part 2

Published in the November/December 2010 issue of Glass Worldwide, the first part of this article looked at all-electric forehearths for the conditioning of volatile glasses such as fluoride opal and borosilicate. In part 2 of this feature, the author considers the conditioning of non-volatile glasses in all-electric forehearths.

Author
G Stuart
Origin
Electroglass, Uk
Journal Title
Glass Worldwide Jan-Feb/2011 49-50, 52