Alkali Sites In Silicate Glasses

The nature of sites occupied by metal ions in glass can be investigated by infrared spectrsocopy. This work presents the results of an infrared reflectance study of alkali silicate glasses of the type zNa20.(1-x)SiO2(0.1

Author
J A Kapoutis Et Al
Origin
Nat Hellenic Research Foundation, Greece
Journal Title
Chimica Chronica, New Series 23 1994 341-346
Sector
Special Glass
Class
S 917

Request article (free for British Glass members)

Alkali Sites In Silicate Glasses
Chimica Chronica, New Series 23 1994 341-346
S 917