Alglass Heat Recover: An Advanced Oxy-Combustion Technology With Heat Recovery For Glass Furnaces Makes Sustainable Performances

Increasing furnace efficiency and reducing NOx & CO2 emissions are today's glassmakers first concerns for being competitive in their market. Innovative solutions are investigated at all levels. They include pretreating the batch to melt glass more efficiently, improving combustion control to reduce NOx & switching to natural gas for lower carbon emissions. For glass production & particularly for flat glass, Air Liquide & AGC Glass Europe have developed recently a highly innovative technology, Alglass Heat recovery to recover most of the heat of the flue gases. This presented four challenges at once: Float furnace conversion to oxy-combustion; Staged oxy-combustion burner technology; Oxygen preheating; & Natural gas preheating. This paper presents the results of the industrial prototype and the various approaches and methodologies that have been launched to make this technical partnership a success. This technology enables reducing operations costs with a profitable investment cost.

Author
Y Joumani Et Al
Origin
Air Liquide R&D
Journal Title
Verre 16 5-6 December 2010 43-48
Sector
General
Class
G 3839

Request article (free for British Glass members)

Alglass Heat Recover: An Advanced Oxy-Combustion Technology With Heat Recovery For Glass Furnaces Makes Sustainable Performances
Verre 16 5-6 December 2010 43-48
G 3839
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.