Air-Cooled Forehearth Electrodes Success For C Glass

In addition to a range of applications in soda-lime and borosilicate glasses, this article reports that VEL 48 air-cooled forehearth electrodes from Grob are now being used successfully in a forehearth for the production of C glass.