Aging Behaviour Of Cuo Modified Batio3 Ceramics

In order to reduce the sintering temperature and enhance the piezoelasticity, a small amount of CuO was added into BaTiO3 during sintering. The aging behaviour of these CuO modified BaTiO3 ceramics was studied systematically. For unpoled ceramic, the P-E loop changes gradually from a normal single-loop curve to a double-loop with aging. Meanwhile, the S-E loop develops gradually from a normal strain curve to one with almost zero strain under electric field below 10kVmm-1. For poled ceramic, it builds a much stronger and more stable internal bias after aging. The P-E loops shift significantly along the electric field and the strain loop shows high asymmetry with one side of high linearity. A dipolar defect model was proposed to explain these aging behaviours. The defect dipoles consisting of Cu2+ occupying B site and oxygen vacancy can re-orientate gradually with time to align with the spontaneous polarisation. Then, the aligned defect dipoles could provide a strong restoring force on the domain wall motion and thus lead to all the observed aging behaviours.

Author
Y Tan Et Al
Origin
Shandong University, Jinan, China
Journal Title
Advances In Applied Ceramics 113 4 2014 223-227
Sector
Glass Ceramics
Class
GC 853

Request article (free for British Glass members)

Aging Behaviour Of Cuo Modified Batio3 Ceramics
Advances In Applied Ceramics 113 4 2014 223-227
GC 853
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.