[Africa] Beta Glass To Expand

African glass container manufacturer Beta Glass has announced plans to further expand its operations in the West Africa sub-region in order to maintain its position in the continent's packaging market. Company Chairman Chris Ogunbanjo said that the decision is necessary due to the impact of the global recession on worldwide economies.