Aesthetical Durability And Designing Products Made By Waste Material

This study was preceded by a study about using waste materials like sewage sludge, fly ash and recycled glass as a partial raw material in bricks and tiles. This paper discusses the aesthetic durability of ceramic building materials using waste as a partial raw material.