Advantage To Manufacturers Of Advanced Ceramics

Resonant Inspection (RI) has recently been introduced for the non-destructive inspection (NDI) of ceramics. While it can also be applied to metals, resonant inspection was developed specifically to detect defects in ceramics. This article shows how RI is being used by many companies to assure the quality of their ceramic products.