Advancing The Prestige Factor With Non-Round Check Detection

Being far less shape-sensitive and thus allowing a wider array of shapes in glass containers, the Non-Round Check Detector (NRCD) and the TIM System provide added incentive for container designers to take every advantage of the design capabilities and superiority of glass. This is especially so with containers for cosmetics, perfumes, premium sauces and single-serve upscale beverages.