Advances In The Annealing Of Hollow Ware, Flatware, And Optical Glasses

This review makes special reference to the opposing views on the optimum annealing schedule for hollow ware, the recent "temnization" principle for flatware, and the importance of annealing blocks of optical glass so that a very uniform refractive index is attained.