Advanced Methods For Chemical Analysis Of Coatings On Glass

Chemical depth profiling analysis of optical coatings require (a) qualification for accurate measurement of the composition of the major elements as well as any dopants or impurities (b) high sensitivity for detection and measurement of ultra low levels of the dopants or impurities and (c) good depth resolution in depth profiling applications for resolving very thin layers or the distribution of various elements within the layers. This paper will first provide an overview of the various microprobe surface analysis techniques for chemical analysis of thin films and compare their relative merits and limitations in terms of sensitivity and quantification. It will then outline the principles a relatively new technique, Sputtered Neutral Mass Spectrometry (SNMS), and discuss its merits for quantitative depth profiling analysis of a wide range of optical coatings.

Author
H Kheyrandish
Origin
Mats, Uk
Journal Title
Proc Icg Extended Abstracts 2 2001 215
Sector
Special Glass
Class
S 2659

Request article (free for British Glass members)

Advanced Methods For Chemical Analysis Of Coatings On Glass
Proc Icg Extended Abstracts 2 2001 215
S 2659
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.