Advanced Fused Cast Refractories

This article gives a brief history of the development of furnace operating conditions and the effects on refractories. It then discusses AZS fused cast refractories and examines the reasons for the development of the new material, Refel 1334S, citing the advantages of using it instead of a standard product.