Advanced Furnace Design For Energy Efficient Glass Melting

In this paper, a new design of a container glass furnace, modeled by the TNO Glass Tank Model is described. The results of the modeling study are discussed and compared with more classical designs.

Author
R A Bauer & A M Lankhorst
Origin
Tno, Netherlands
Journal Title
Int Glass Journal No 102 1999 128-131
Sector
General
Class
G 2169