Adherent Antireflection Coatings On Borosilicate Glass For Solar Collectors

This paper describes the successful development of a porous SiO2-containing antireflective coating ~110nm thick, which was applied by a sol-gel dip coating process and which increased light transmittance by up to 5%. Previous antireflective coatings did not have sufficient adhesion strength and resistance to wiping on borosilicate glass, so that they do not withstand the rough operating conditions seen in practice. The essential component enhancing the stability of the coating turned out to be H3PO4 which is added to the dropping solution. After baking the sol-gel layers for 1h at 500 deg C, both Na and P concentration peaks develop at both sides of the interface, obviously forming Na2O phosphosilicate glasses, assuring a high long term stability between glass and layer.

Author
G Helsch Et Al
Origin
University Clausthal, Germany
Journal Title
Glass Tehcnology 47 5 2007 153-156
Sector
Special Glass
Class
S 3225

Request article (free for British Glass members)

Adherent Antireflection Coatings On Borosilicate Glass For Solar Collectors
Glass Tehcnology 47 5 2007 153-156
S 3225
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.