Act Platinum Coatings - Their Role In Stabilising Glass Production Processes

This paper describes the use of thin, thermally sprayed platinum coatings to protect standard glass forming and containment ceramics. The paper discusses the properties of ACT Pt coatings and concludes that their durability cannot be explained by a simple extrapolation from the behaviour of thicker, free-standing Pt claddings. The reconfiguration of Pt as an ACT coating, therefore, provides a cost effective method of protecting glass contact ceramics, increasing component lifetimes and stabilising glass production processes.

Author
M Doyle Et Al
Origin
Johnson Matthey Noble Metals, Uk
Journal Title
Int Glass Journal No 102 1999 89-93
Sector
General
Class
G 2167

Request article (free for British Glass members)

Act Platinum Coatings - Their Role In Stabilising Glass Production Processes
Int Glass Journal No 102 1999 89-93
G 2167
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.