Acid-Alkali Modelling Of Turbulent Diffusion Flames

The experimental technique of acid-alkali modelling within a small scale replica of a furnace, the aspects of combustion that can be studied, and their influence on the performance of the furnace are described with particular reference to its application to a glass melting tank.