Accurate Conductivity Cell For Molten Glasses And Salts

A cell for measuring absolute conductances of glass and salt melts is described.

Author
F G K Baucke Et Al
Origin
Schott Glaswerke
Journal Title
Glastech Ber 1989 62 4 122-126
Sector
General
Class
G 247

Request article (free for British Glass members)

Accurate Conductivity Cell For Molten Glasses And Salts
Glastech Ber 1989 62 4 122-126
G 247