Accelerating The Design Of Functional Glasses Through Modeling

Functional glasses play a critical role in current and developing technologies. These materials have traditionally been designed empirically through trial-and-error experimentation. However, here we report recent advancements in the design of new glass compositions starting at the atomic level, which have become possible through an unprecedented level of understanding of glass physics and chemistry. For example, new damage-resistant glasses have been developed using models that predict both manufacturing-related attributes (e.g., viscosity, liquidus temperature, and refractory compatibility), as well as the relevant end-use properties of the glass (e.g., elastic moduli, compressive stress, and damage resistance). We demonstrate how this approach can be used to accelerate the design of new industrial glasses for use in various applications. Through a combination of models at different scales, from atomistic through empirical modeling, it is now possible to decode the “glassy genome” and efficiently design optimized glass compositions for production at an industrial scale.

Author
J C Mauro
Origin
Corning Glass
Journal Title
Chemistry Of Materials 28 12 2016 4267-4277
Sector
General
Class
G 4524

Request article (free for British Glass members)

Accelerating The Design Of Functional Glasses Through Modeling
Chemistry Of Materials 28 12 2016 4267-4277
G 4524
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.