Absorption And Photoluminescence Of Pr3+-Doped Fluorophosphate Glasses

The optical characteristics of six newly developed fluorophosphate glasses are briefly reported.

Author
A V Ranga Reddy Et Al
Origin
Sri Venkateswara University, India
Journal Title
Phys Chem Glasses 1991 32 6 263 - 265