About The Origin Of Non-Newtonian Flow Of Glass Melts

A recently developed flow equation is briefly presented. A parallel exists to a certain degree to the Maxwellian relaxation theorem; however, characteristic differences will be pointed out.

Author
R Bruckner
Origin
Inst Fur Nichtmetallische Werkstoffe, Tu Berlin
Journal Title
5Th Int Otto Schott Colloquium, Jena, July 1994 161-166