Ab Initio Based Studies Of Borate Glasses

Ab initio calculations of boric oxide are used to parameterize a classical model of the interactions between boron and oxygen. This model yields a structure that agrees extremely well with all known measurements of the properties of vitreous boric oxide, but the concentration of boroxol rings is nearly an order of magnitude less than commonly accepted. Quantitative Raman measurements using calibrated samples of boroxol ring concentrations yield a quantitative measurement of the ring concentration in vitreous boric oxide in close agreement with the simulation.

Author
M Teter
Origin
Corning New York
Journal Title
Corning Research 1997 135-144
Sector
Special Glass
Class
S 1453

Request article (free for British Glass members)

Ab Initio Based Studies Of Borate Glasses
Corning Research 1997 135-144
S 1453
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.