Ab Initio Based Studies Of Borate Glasses

Ab initio calculations of boric oxide are used to parameterize a classical model of the interactions between boron and oxygen. This model yields a structure that agrees extremely well with all known measurements of the properties of vitreous boric oxide, but he concentration of boroxol rings is nearly an order of magnitude less that commonly accepted. Quantitative Raman measurements using calibrated samples of boroxol ring concentrations yield a quantitative measurement of the ring concentration in vitreous boric oxide in close agreement with the simulation.

Author
M Teter
Origin
Corning Inc, New York, Usa
Journal Title
Proc Second Int Conf Borate Glasses, Crystals & Melts 407-416
Sector
Special Glass
Class
S 3670

Request article (free for British Glass members)

Ab Initio Based Studies Of Borate Glasses
Proc Second Int Conf Borate Glasses, Crystals & Melts 407-416
S 3670
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.