57Fe Mossbauer Spectroscopy And Magnetic Susceptibility Of Iron Alkali Silicate Glasses

The structure and properties of iron alkali silicate glasses depend to a large extent on the structural role of iron such as its valence state and coordination. Both are a function of the oxygen fugacity, the total amount of iron present and the amount and type of alkalis as well as pressure, temperature and quenching rate. This paper addresses the structural role of iron as a function of alkalis and alkali content.

Author
D J M Burkhard
Origin
University Of Maburg, Germany
Journal Title
Phys Chem Glasses 38 6 1997 317-322
Sector
Special Glass
Class
S 1308

Request article (free for British Glass members)

57Fe Mossbauer Spectroscopy And Magnetic Susceptibility Of Iron Alkali Silicate Glasses
Phys Chem Glasses 38 6 1997 317-322
S 1308
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.