3-D Printed Bioceramic Composite Offers Flexible New Hope For Bone Replacement

Researchers at Northwester University (Evanston, Ill), report they have developed a hyperelastic material that can be 3-D printed into a potential bone replacement scaffold. The material is a 3-D printable ink that consists of hydroxyapatite and a biodegradable, biocompatible polymer binder in a solvent that evaporates during printing. The liquid ink can be rapidly 3-D printed at room temperature. The key to the new material is its Goldilocks combination of materials to provide strength and flexibility.

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 96 1 2917 23
Sector
Special Glass
Class
S 4342

Request article (free for British Glass members)

3-D Printed Bioceramic Composite Offers Flexible New Hope For Bone Replacement
Am Ceram Soc Bull 96 1 2917 23
S 4342
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.