29Si Mas Nmr Studies Of Alkali Silicate Oxynitride Glasses

Magic angle spinning nuclear magnetic resonance has been applied to study the structural effect of nitrogen incorporation into glasses.

Author
W Hater, W Muller-Warmuth, G H Frischat
Origin
Westfalische Wilhelms-Universitat, Technische Universitat Clausthal
Journal Title
Glastech Ber 1989 62 9 328-334