100% Oxy-Fuel Firing: The Real Story

Many companies are presently considering 100% oxy-fuel firing of glass melting furnaces. The most recent conversions in Europe, North America and Southeast Asia have been driven by both environmental regulations and the need for increased production. Virtually all segments of the glass industry in the US have now implemented 100% oxy-fuel combustion technology. This paper describes Combustion Tec's experience in various segments of the glass industry for design and implementation of Primefire oxy-fuel technology. To begin, experience has given valuable insight in how a converison affects the various personnel throughout the glass plant. This paper identifies some of the issues for those planning to convert.

Author
M J Damsell Et Al
Origin
Combustion Tech Inc, Usa
Journal Title
Glass Technology 37 4 1996 114-117
Sector
General
Class
G 1486

Request article (free for British Glass members)

100% Oxy-Fuel Firing: The Real Story
Glass Technology 37 4 1996 114-117
G 1486
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.